Collaborations and top research areas from the last five years
Recent external collaboration on country/territory level. Dive into details by clicking on the dots or
-
Oxygen-driven de-alloying of Fe-14Cr-12Ni-10Mn-3Cu-2.5Al-1Nb austenitic steel at 500 °C in static Pb-Bi eutectic with concentration of dissolved oxygen alternating from ∼10-6 to 10-9 mass% for 10000 h
Tsisar, V., Stergar, E., Gavrilov, S., Maia, E. L., Van Renterghem, W., Louette, P. & Lucas, S., Mar 2025, In: Corrosion Communications. 17, p. 1-11 11 p.Research output › peer-review
Open Access -
Early stages of liquid metal corrosion - Austenitic stainless steel 316L exposed to liquid lead-bismuth eutectic
Lopes Maia, E., Gavrilov, S. & Tsisar, V., 11 Oct 2024, VUB - Vrije Universiteit Brussel. 249 p.Research output
Open AccessFile51 Downloads (Pure) -
Early stages of liquid-metal corrosion on pre-oxidized surfaces of austenitic stainless steel 316L exposed to static Pb-Bi eutectic at 400 °C
Lopes Maia, E., Gavrilov, S., Tsisar, V., Baert, K. & De Graeve, I., Feb 2024, In: Corrosion Science. 227, 13 p., 111680.Research output › peer-review
-
Oxygen-enhanced dissolution corrosion of austenitic stainless steel 316 L in static lead-bismuth eutectic at 500 °C
Lopes Maia, E., Tsybanev, A., Gavrilov, S., Tsisar, V., Lim, J. & De Graeve, I., 1 Aug 2024, In: Corrosion Science. 236, 9 p., 112224.Research output › peer-review
-
Prediction of ‘effective’ corrosion rates by in-situ internal pressure creep testing in LBE for Ti-stabilised DIN 1.4970 (15-15Ti) austenitic stainless steel cladding tubes
Holmström, S., Stergar, E., Gavrilov, S., Tsisar, V., Joris, J. & Lopes Maia, E., 5 Mar 2024, In: Materials At High Temperatures. 41, 2, p. 294-301 8 p.Research output › peer-review
Open Access