title = "LOTION 2 - Tensile tests op AISI 316 L and T19 weld specimens irradiated at 315 K: PSM 1-3 - Final report",
abstract = "In the framework of the CEC-DGXII-Fusion NET Technology Programme, AISI 316L base material and TIG Metal Deposit specimens have been irradiated at a temperature of about 350 K, up to 5 dpa. Irradiated und irradiated specimens have been tensile tested at 25°C, 250°C and 450°C. At all temperatures important irradiation hardening is observed. The TIG Metal Deposit exhibits lower ductility.",