Abstract
Tungsten has been selected as the plasma-facing material for ITER's first wall and divertor. Plasma-facing components for fusion environments must withstand extreme thermal and mechanical loads, particularly during transient events such as edge localized modes. These events generate significant thermal gradients and large mechanical loads, subjecting the material to a wide range of strain rates. Failure of these components could interrupt the reactor operation and potentially damage the surrounding systems, including the test blanket modules. To evaluate the mechanical integrity of material under such conditions, tensile tests were conducted on two ITER-specification tungsten grades for divertor components at temperatures between 250 °C and 550 °C and strain rates ranging from 6.4 × 10−4 to 6.4 × 10−2 s−1. The goal of the study is to determine the viscoplastic behavior of tungsten and to assess the impact of temperature and strain rate on its mechanical performance. The fracture surfaces and initial microstructures were analyzed by scanning electron microscopy. The results reveal a clear strain rate dependency of the strength and ductility, with a ductile-to-brittle transition at lower temperatures and higher strain rates. Differences in performance between the two tungsten grades are linked to microstructural features and impurity content. These findings highlight the impact of the processing route and of initial microstructure on the mechanical performance of plasma facing components.
| Original language | English |
|---|---|
| Article number | 107811 |
| Number of pages | 10 |
| Journal | International Journal of Refractory Metals and Hard Materials |
| Volume | 139 |
| DOIs | |
| State | Published - Sep 2026 |
ASJC Scopus subject areas
- Ceramics and Composites
- Mechanics of Materials
- Mechanical Engineering
- Metals and Alloys
- Materials Chemistry
Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver