TY - JOUR
T1 - Unveiling the origin of low-dose brittleness in W/Cu laminates
T2 - interfacial defect complexes and their role in irradiation hardening
AU - Li, Yifan
AU - Pang, Gang-Qiang
AU - Li, Yu-Hoa
AU - Niu, Yu-Ze
AU - Terentyev, Dmitry
AU - Zhou, Hong-Bo
AU - Lu, Guang-Hong
N1 - Score=10
Publisher Copyright:
© 2026 Elsevier B.V.
PY - 2026/9
Y1 - 2026/9
N2 - Since W/Cu laminates have great potential application in the plasma-facing components, understanding their response to high-energy neutron is therefore an essential requirement. Recent experiments have reported unexpected brittle fracture in W/Cu laminates following low-dose neutron irradiation, yet the underlying mechanism remains unclear. Here, we systematically investigate the behaviors of point defect in W(110)/Cu(111) interface and its influence on the evolution of displacement damage as well as the hardness increase in W using the multi-scale simulations. It is found that the W/Cu interface can serve as the effective trapping center for point defects in both W and Cu. Intriguingly, the defect segregation into the interface substitutes the Cu atoms, which further traverse the interface and enter the W side. Due to the different atomic radius and/or electron structure, Cu atoms interact strongly with self-interstitial atoms (SIAs) and also bind with vacancies in W, thereby forming Cu-SIA and Cu-Vac complexes. Especially for the interstitial Cu, its diffusion energy barrier is only 0.34 eV, corresponding to the dominant method for Cu diffusion in irradiated W. Combining the atomistic parameters with object kinetic Monte Carlo (OKMC) simulations, we demonstrate that the Cu addition increases the number of surviving defects in W under neutron irradiation. This can be attributed to the strong attraction between Cu and SIAs, resulting in the formation of immobile Cu-SIA complexes and suppressing the vacancy-interstitial recombination. Such effect largely depends on the Cu insert rates and temperatures, and also leads to an extra contribution on the irradiation hardening of W. Our findings provide a plausible explanation for experimental observations and highlight the crucial role of interfaces in governing material responses to neutron irradiation.
AB - Since W/Cu laminates have great potential application in the plasma-facing components, understanding their response to high-energy neutron is therefore an essential requirement. Recent experiments have reported unexpected brittle fracture in W/Cu laminates following low-dose neutron irradiation, yet the underlying mechanism remains unclear. Here, we systematically investigate the behaviors of point defect in W(110)/Cu(111) interface and its influence on the evolution of displacement damage as well as the hardness increase in W using the multi-scale simulations. It is found that the W/Cu interface can serve as the effective trapping center for point defects in both W and Cu. Intriguingly, the defect segregation into the interface substitutes the Cu atoms, which further traverse the interface and enter the W side. Due to the different atomic radius and/or electron structure, Cu atoms interact strongly with self-interstitial atoms (SIAs) and also bind with vacancies in W, thereby forming Cu-SIA and Cu-Vac complexes. Especially for the interstitial Cu, its diffusion energy barrier is only 0.34 eV, corresponding to the dominant method for Cu diffusion in irradiated W. Combining the atomistic parameters with object kinetic Monte Carlo (OKMC) simulations, we demonstrate that the Cu addition increases the number of surviving defects in W under neutron irradiation. This can be attributed to the strong attraction between Cu and SIAs, resulting in the formation of immobile Cu-SIA complexes and suppressing the vacancy-interstitial recombination. Such effect largely depends on the Cu insert rates and temperatures, and also leads to an extra contribution on the irradiation hardening of W. Our findings provide a plausible explanation for experimental observations and highlight the crucial role of interfaces in governing material responses to neutron irradiation.
KW - Tungsten-copper
KW - Interfacial diffusion
KW - Irradiation defects
KW - Multiscale simulation
UR - https://www.scopus.com/pages/publications/105041860882
U2 - 10.1016/j.jnucmat.2026.156819
DO - 10.1016/j.jnucmat.2026.156819
M3 - Article
SN - 0022-3115
VL - 631
JO - Journal of Nuclear Materials
JF - Journal of Nuclear Materials
M1 - 156819
ER -